Vinyl Ester Resin Specification List
Resin name | Type | Viscosity cPs@25℃* | Gel time Min @25℃* | Tensile str. MPa | El. at break % | HDT ℃ | Remarks |
711 | BPA-VE | 250-450 | 15-25 | 80-95 | 5.0-6.0 | 100-106 | Premium grade, 10 months shelf life |
722 | BPA-VE | 400-600 | 20-30 | 70-80 | 3.0-4.0 | 125-135 | Cost effective, high temperature and corrosion resistant |
707H | Brominated VE | 300-450 | 15-25 | 78-90 | 4.0-6.0 | 108-115 | Highest bromine content for most critical fire retardant requirements. |
707A | Brominated VE | 300-450 | 15-25 | 78-90 | 4.0-6.0 | 106-110 | High fire retardant performance, cost effective |
707N | Novalac Brominated VE | 300-450 | 15-25 | 70-80 | 3.5-5.0 | 128-137 | Fire-retardant, heat resistant and corrosion resistant |
770 | Novolac VE | 230-370 | 11-19 | 75-90 | 3.0-4.0 | 145-150 | Resistant to high temperature |
780 | Novolac VE | 230-370 | 15-25 | 78-90 | 2.5-3.5 | 160-166 | Resistant to high temperature, solvents and oxidizing agents. Excellent mechanical properties. HDT range from 145-210 deg C. |
780HT | Novolac VE | 600-900 | 15-25 | 70-80 | 2.0-3.0 | 200-210 | |
780HS | Novolac VE | 250-550 | 15-25 | 80-90 | 3.0-4.0 | 170-175 | |
790 | PU modified | 350-600 | 15-25 | 60-70 | 12.0-13.0 | 80-88 | Largely improve the flexibility, tensile strength and impact strength for FRP gas cylinder. |
791 | Elastomer modified | 300-450 | 15-25 | 63-80 | 10.0-12.0 | 75-85 | Improved bonding strength to steel, aluminum, concrete; abrasion and mechanical stress resistant. |
901 | Epoxy VE | 250-450 | 15-35 | 75-95 | 5.0-6.0 | 105-110 | Excellent corrosion resistance,good mechanical strength, superior toughness with excellent fatigue resistance. |