Resin name | Type | Viscosity cPs@25℃ | Gel time Min @25℃* | Tensile str. MPa | El. at break % | HDT ℃ | Remarks | Approval |
11VP | BPA-VE | 150-250 | 30-60 | 80-95 | 4.0-6.0 | 95-105 | Low viscosity, peak exotherm and shrinkage for RTM | Loyd’s Register |
11TP | 300-500 | 10-20 | 75-85 | 4.0-5.0 | 95-105 | Thixotropic version for hand lay-up and spray up | ||
9709VP | Orthe | 150-250 | 30-60 | 70-75 | 3.0-4.0 | 75-85 | Low viscosity, peak exotherm and shrinkage for RTM | |
9709TP | 300-600 | 10-40 | 65-75 | 3.0-4.0 | 75-85 | Thixotropic version for hand lay-up and spray up | ||
9406VP | Iso | 180-220 | 30-60 | 60-70 | 2.5 | 85-95 | Low viscosity, peak exotherm and shrinkage for RTM | |
9406TP | 300-500 | 10-20 | 70-80 | 3.0-4.0 | 90-100 | Thixotropic version for hand lay-up and spray up | ||
30-200P | VE | 150-250 | 60-180 | 85-95 | 4.0-6.0 | 105-110 | Longer gel time than MFE 11VP, for large FRP infusion | GL |
9190P | Orthe | 100-200 | 30-180 | 70-80 | 3.0-5.0 | 80-100 | Low viscosity, long gel time | |
707 | Halogen free VE | 300-450 | 8-16 | 78-90 | 4.0-6.0 | 108-115 | L.O.I.=28(Resin casting), 38(FRP laminate). UL-94 V-0. BS476-6 class 0, DIN 5510 S4/ST2/SR2 when ATH added. | CCS |