AR roving 16.5%
  2018/12/14| View:933

ARG fiber ZrO2 min content is 16.7%, over the EU BSEN15422:2008 and USA ASTMC 1666 standard, ZrO2 content higher, alkali-resistance performance and durability is better.

 

1:A TYPICAL COMPOSITION OF ARG FIBER IS SHOWN AS FOLLOWS:

 

Aggregates

SiO2

ZrO2

Al2O3

CaO

Na2O

K2O

Standard %

60-62

16.7-20

0.3-0.8

0.5-5.6

14-17

0-2

 

 

We guarantee that Zro2 content of ARG glass fiber (roving and chopped strand) can remain unchanged over 30 years.